The slide plate is made of ASTM A-297-HH heat-resistant steel material, precision cast with coated sand core, and optimized for performance through solution heat treatment. Its recommended long-term use temperature does not exceed 1250 ℃.
The slide plate is made of ASTM A-297-HH heat-resistant steel material, precision cast with coated sand core, and optimized for performance through solution heat treatment. Its recommended long-term use temperature does not exceed 1250 ℃.
The rod drop seal material is Q235+65Mn. During the casting process, the product undergoes surface paint rust prevention treatment,. The appearance dimensions of the product are also 100% size inspected.
The end slide rail material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The central slide rail material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The head slide rail material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The end casting material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The front pllate material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The running wheel assy material is 42CrMo. During the casting process, the product undergoes surface medium frequency quenching heat treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.
The spring seal assy material is 55#. During the casting process, the product undergoes surface paint rust prevention treatment, as well as magnetic particle inspection and ultrasonic testing. The appearance dimensions of the product are also 100% size inspected.